Where do you buy aluminum oxide?
Alecia
Aluminum Oxide
Moderators: Brad Walker, Tony Smith
-
- Posts: 108
- Joined: Mon Aug 25, 2003 12:35 am
- Location: outside of Dallas TX
Aluminum Oxide
Alecia Helton
Wear Original Wonders!
Carrollton TX
Wear Original Wonders!
Carrollton TX
Locally
I just looked in the phone book under Sand Blasting
called around to get the best prices.
I buy the minimum 50# for $25
http://www.gnpltd.com/
It is local for me ...but they do ship
called around to get the best prices.
I buy the minimum 50# for $25
http://www.gnpltd.com/
It is local for me ...but they do ship
-
- Posts: 16
- Joined: Tue Mar 11, 2003 10:33 am
- Location: Desert Southwest
I just talked to a guy who makes stone monuments. He told me about something called "Banding Sand" and he says it's a very sharp, efficient abrasive. Cheap, too. I was talking to him about sandblasting a photographic image and he says I should use this "banding sand".
It's 0000 (four O s) size particle, said if the particle was any smaller it would be dust. He get's it from Bicknell Supply somewhere in Georgia.
Call 1-800-241-7105.
I'm going to try it as soon as I can get it.
Oh yea, He says he uses tons of it and gets it for about $7.50/ 100 lbs.
It's 0000 (four O s) size particle, said if the particle was any smaller it would be dust. He get's it from Bicknell Supply somewhere in Georgia.
Call 1-800-241-7105.
I'm going to try it as soon as I can get it.
Oh yea, He says he uses tons of it and gets it for about $7.50/ 100 lbs.
-
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada