Page 1 of 1
Sanding sponges - and now angle grinders and pads.
Posted: Sat Mar 06, 2004 5:06 am
by Stuart Clayman
What is the order of the color of the sponges from roughest to smoothest?
Posted: Sat Mar 06, 2004 6:11 am
by Lauri Levanto
Mine are of two brands with different color coding!
A rule of thumb SEEMS TO BE that
coarse pads have small patches of abrasive
fine grits come with larger patches.
-lauri
Re: Sanding sponges
Posted: Sat Mar 06, 2004 11:38 am
by Brad Walker
Stuart Clayman wrote:What is the order of the color of the sponges from roughest to smoothest?
Depends on the brand.
Posted: Sat Mar 06, 2004 12:00 pm
by Stuart Clayman
Not sure what brand I have. They came as a set so I assuem that they are the same manufacturer.
The colors are Green, black, yellow, red and white. The green is the roughest, then the black, and the white I think if the finest. I am not sure between the yellow and red.
Posted: Sat Mar 06, 2004 12:10 pm
by Rebecca M.
My yellow one says 320. The ink is gone from all the rest and I don't know what brand they are either.
Posted: Sat Mar 06, 2004 12:12 pm
by Stuart Clayman
Mine do not have any writing on them.
Posted: Sat Mar 06, 2004 12:15 pm
by charlie holden
If they are 3M they are on this page:
http://www.granquartz.com/hand.htm
ch
Posted: Sat Mar 06, 2004 12:23 pm
by Stuart Clayman
Thanks Charlie,
That was it. So, I have the 60, 120, 220, 400 and the 800. I also see there is a 600 and a 1800. Does anyone use these 2?
Stuart
Posted: Sat Mar 06, 2004 12:27 pm
by Brad Walker
Stuart Clayman wrote:That was it. So, I have the 60, 120, 220, 400 and the 800. I also see there is a 600 and a 1800. Does anyone use these 2?
The really fine grits aren't used on glass, just granite and things like that. Remember, most of these pads are probably bought for polishing rocks, not for working with glass.
Posted: Sun Mar 07, 2004 12:53 pm
by Lauri Levanto
I have only two hand pads.
The set rotating pads I have for angular grinder
goes to 1800 (orange).
It gives a nice polish to glass, but not perfect gloss.
I suppose pumice and cerium are unavoidable steps.
One should use the pads in binary order.
First coarse, then double the grit and work until
magnifying glass reveas no coarse markings.
Double the grit again etc.
Remember to wash the glass, hands and the workin area
between each grit.
Use some pressure on the pads, and plenty of water.
A thin white sludge is what you want to see.
-lauri
Posted: Sun Mar 07, 2004 1:51 pm
by Stuart Clayman
lauri wrote:
The set rotating pads I have for angular grinder
goes to 1800 (orange).
-lauri
If I understand you correctly you have a angular grinder, I assume like the one in the link below, that has a set of rotating pads that goes to 1800. Where does one get diamond pads to fit those in the US? Anyone knows?
http://cgi.ebay.com/ebaymotors/ws/eBayI ... 2464724511
Posted: Sun Mar 07, 2004 7:02 pm
by charlie holden
Stuart Clayman wrote:lauri wrote:
The set rotating pads I have for angular grinder
goes to 1800 (orange).
-lauri
If I understand you correctly you have a angular grinder, I assume like the one in the link below, that has a set of rotating pads that goes to 1800. Where does one get diamond pads to fit those in the US? Anyone knows?
http://cgi.ebay.com/ebaymotors/ws/eBayI ... 2464724511
Better angle grinders have water feeds through the shaft. Go back to the link I posted before and click around.
ch
Posted: Mon Mar 08, 2004 12:38 pm
by charlie
Stuart Clayman wrote:lauri wrote:
The set rotating pads I have for angular grinder
goes to 1800 (orange).
-lauri
If I understand you correctly you have a angular grinder, I assume like the one in the link below, that has a set of rotating pads that goes to 1800. Where does one get diamond pads to fit those in the US? Anyone knows?
http://cgi.ebay.com/ebaymotors/ws/eBayI ... 2464724511
the granite polishing industry has used these forever. i just had a granite slab edge polished. wish i worked there to just play with the tools. look at headstone or countertop tooling. poke around at
http://www.granitecitytool.com/
Posted: Mon Mar 08, 2004 1:45 pm
by gthomson
Stuart Clayman wrote:
If I understand you correctly you have a angular grinder, I assume like the one in the link below, that has a set of rotating pads that goes to 1800. Where does one get diamond pads to fit those in the US? Anyone knows?
http://cgi.ebay.com/ebaymotors/ws/eBayI ... 2464724511
Well, I've got one of those, and I'd like to know as well. Would silicon carbide discs be OK?
Which brings me to a related question: what other 'home shop' tools can be pressed into service temporarily/cheaply untill the specialized stuff gets acquired? I've got a bench grinder, metal lathe, drill press, router, dremel, and all the typical things like drills.
Thanks,
Glenn
Posted: Mon Mar 08, 2004 2:25 pm
by Jack Bowman
Stuart asks...
If I understand you correctly you have a angular grinder, I assume like the one in the link below, that has a set of rotating pads that goes to 1800. Where does one get diamond pads to fit those in the US? Anyone knows?
Stuart,
http://www.granitecitytool.com/stone-to ... catnum=252
Jack
Posted: Mon Mar 08, 2004 2:35 pm
by Stuart Clayman
Ok, now that I know that I can get disks for it.. and I konw that there are some people that use that type of grinder for glass. What do ya'll use it for? Doing a buff job on it? Sorry it reminds me of a car buffer.
Stuart
Posted: Wed Mar 10, 2004 2:30 pm
by Lauri Levanto
Hi Stuart
The disks I have are of Telum Brand,
most propably US made.
The grinder is of that type, a bit stronger that car polishing tools.
In fact I use the pads on a handheld drill
- to get variable speed control. They work best in moderate speed.
I do grind of flashings, sometimes level out
the base of a cast piece.
I am still testing with the fine applications like polishing.
They can be used for larger flat areas, so my style of sculpting has to take it in consideration.
They work pretty fast when cleaning of needling of flat pieces.
There are similar disks for a Dremel-type tool, maybe
2" diam. Mine are 5". That source carries
small cylindrical pads for Dremel, too.
Hope to get hands on such.
-lauri
Posted: Fri Mar 12, 2004 11:17 am
by StaceyG
Does anyone know where to get the 3Mâ„¢ Diamond Files and pads without having to order them on the internet. Does someplace like Home Depot or Lowes carry them? Or should I go to a specialty shop of some kind?
Thanks,
Stacey
Posted: Fri Mar 12, 2004 11:30 am
by charlie
woodworking specialty stores