Bellknap
Posts: 26
Joined: Tue Feb 10, 2004 10:20 am
Location: Columbus, Ohio

My first fuse item photos

Postby Bellknap » Mon Mar 08, 2004 5:53 pm

Well I have learning a ton from all of you....a big thank you to all.
I have posted my second, third and fourth fuse. The fish is the last one, the photo doesn't show well, it is actually a bright orange clownfish with a lifted fin. The aqua is a small bowl and the geometric bright blue is a square slump mold. All are 6" or less. Again my sincerest thanks for all that have answered by questions....Lydia of Ohio ImageImageImage
Here is the website is you are perhaps interested in larger photos.

http://community.webshots.com/album/124032185rNcvJo?208

molly
Posts: 69
Joined: Tue Jul 15, 2003 7:38 pm

Postby molly » Mon Mar 08, 2004 8:36 pm

WOW! And you say you are just a "beginner"???? Seems to me you are doing really well! Beautiful work~......keep it up, and you will really GO places!!!

Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Postby Paul Tarlow » Mon Mar 08, 2004 8:48 pm

You're off to an awesome start -- keep it up :)

Stuart Clayman
Posts: 224
Joined: Mon Mar 31, 2003 12:35 pm
Location: Virginia
Contact:

Postby Stuart Clayman » Mon Mar 08, 2004 8:53 pm

Wow, these are great, not just for a beginner. I am taking a break from a beginner class that I am teaching tonight. At first I thought about showing the students what a beginner can do, but on second thought I don't want to discourage them. These are wonderful.

Stuart
Last edited by Stuart Clayman on Tue Mar 09, 2004 12:40 am, edited 1 time in total.
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman

Cynthia

Re: My first fuse item photos

Postby Cynthia » Mon Mar 08, 2004 8:53 pm

Bellknap wrote:ImageImageImage
Here is the website is you are perhaps interested in larger photos.

http://community.webshots.com/album/124032185rNcvJo?208


Lydia, these are great. Nice composition on the blue framed piece.

How did you get these thumbnails to show up? Are they on a webshots site location for thumbnails? Are these being shown from a webshots site.? I haven't found a way to get webshots to allow posting an image hosted on their site...But it appears that you have. :shock:

Bellknap
Posts: 26
Joined: Tue Feb 10, 2004 10:20 am
Location: Columbus, Ohio

Photo posting...

Postby Bellknap » Mon Mar 08, 2004 9:41 pm

Cynthia, well I found out by trial and error. After you write your message, hit the img button once. Then while you are looking at the photo you want in webshots left click it, go to properties and copy/paste the entire description line into your message, then click the img box above again. If you press preview you can tell if you did it right or not. Hope this is not clear as mud! Lydia

Cynthia

Postby Cynthia » Tue Mar 09, 2004 2:25 pm

Image

How crazy is that?

I think it worked.

Thanks Lydia.

Bellknap
Posts: 26
Joined: Tue Feb 10, 2004 10:20 am
Location: Columbus, Ohio

Postby Bellknap » Tue Mar 09, 2004 2:29 pm

Cynthia,
don't you love it when something works! I always say if I learn something today I can go home, so now you can go home. Lydia


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 37 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com