Postby dan001 » Fri Mar 12, 2004 7:58 pm

I am looking for some blank decal paper that we could silkscreen print on and then re sell to local glass shop.

Any idea of a suppliers

Thanks

Dan
L&D Design

Luiza
Posts: 81
Joined: Sun Mar 09, 2003 4:50 pm
Location: Rio de Janeiro / Brazil

Postby Luiza » Fri Mar 12, 2004 8:49 pm

Hi Dan
I think you will find it at
http://www.beldecal.com/decals.cfm
Luiza

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Sat Mar 13, 2004 12:33 am

L. Reusche in Colorado sells it.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 26 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com