Postby Stuart Clayman » Fri Mar 19, 2004 8:22 pm

I got an e-mail today on a different glass board that I am on.. it was from: "barbs" <barb_d_@webtv.net>

Here is the message: hi, my name is Barb. Back in June of 2003 I moved from Dyer, Indiana
to Salem, Ohio. I was a member of the Crete Lion Club. I transferred
to the Salem Lions Club. Right now I am in the process of moving
from
Salem, back to the area of Crete, Illinois.
We have a recycling center that takes in sometimes large quantities of
green and blue glass. I am trying to find a way to recycle these
bottles as we don't have a buyer for them at this time.
I know the green is hard to melt down but I was thinking maybe members
of this forum might have some suggestions because the purpose of having
the center is so we don't put as much in the dumpster.
I have contacted some companies that make products out of recycled
green
and blue glass.....but most of them are too far away for it to be
convenient.
looking forward to hearing from you.....


Did not know if anyone would be interested.....
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Postby Lynn g » Sat Mar 20, 2004 3:46 am

Stuart, tell Barb to try http://www.greenglass.com in Schofield, Wis; they make glassware from bottles and contract with recycling centers. Also http://www.ecofriendlyflooring.com, located in Madison, Wis makes recycled glass tiles.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

barbs

recycled glass in crete

Postby barbs » Sat Mar 20, 2004 12:20 pm

I did contact both of them and was told to expect a phone call this past week.....but as of yet, neither one called.

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Postby Lynn g » Sat Mar 20, 2004 6:17 pm

barbs - I hear you! I have spent nearly a month trying to get estimates from printers for a calendar our animal center is trying to put together...only one has responded without follow-up; the rest either have not gotten back to me in spite of many promises, or have needed multiple follow-ups! They say patience is a virtue...I certainly hope so!
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 15 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com