carol nahoom
Posts: 17
Joined: Mon Nov 03, 2003 8:12 am
Location: Crawfordville, Florida

pot melt info wanted

Postby carol nahoom » Sun Mar 21, 2004 8:47 am

Where can I find a tutorial for making the pot melts? I checked the archive but cannot find a "how to".

thanks
carol
Last edited by carol nahoom on Sun Mar 21, 2004 5:11 pm, edited 1 time in total.

Randy W
Posts: 91
Joined: Sun Mar 09, 2003 6:19 pm
Location: Racine, Wisconsin

Postby Randy W » Sun Mar 21, 2004 2:26 pm

When injustice becomes law, rebellion becomes duty.

AZ gram
Posts: 31
Joined: Sat Jan 31, 2004 8:44 pm
Location: Phoenix, AZ
Contact:

Thank you, thank you....

Postby AZ gram » Sun Mar 21, 2004 3:18 pm

It is soooooooo generous of you to share your technique. The photos and descriptions are clear and inspiring. Your magnet was one of my favorites.

carol nahoom
Posts: 17
Joined: Mon Nov 03, 2003 8:12 am
Location: Crawfordville, Florida

Postby carol nahoom » Sun Mar 21, 2004 5:04 pm

Randy..........awesome!! Really...thank you!

Carol

Lauralei
Posts: 37
Joined: Sat Mar 29, 2003 9:35 am
Location: Annapolis, Md.

Postby Lauralei » Sun Mar 21, 2004 6:28 pm

Randy !
Thanks for the detailed 'how to" your magnet was one of the most amazing! Thanks so much for sharing! So you don't have to put kilnwash on the pot interiors at all huh?
Lauralei

froggee501
Posts: 43
Joined: Thu Feb 26, 2004 6:45 pm
Location: Portamazoo, MI

Postby froggee501 » Sun Mar 21, 2004 8:31 pm

while I've never potmelted before, the impression I get is that no, you don't need to kiln wash the pot interior... after all, you are melting out of it, and what little is left behind isn't worth saving, and using kiln wash inside the pot may even contaminate your potmelt.

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Postby Lynn g » Mon Mar 22, 2004 1:05 am

Randy, this is so cool! Thank you! I have been curious about what I've read on the board about pot melts (and the maglesses I received) but haven't had time to hunt through the archives. Now you have saved me all that time and effort with a beautifully clear explanation. You should write a book!

I'm serious...maybe something along the lines of "Fun Things to Do with Your Kiln Without a Major Investment in Complicated Equipment". ("Fusing for Dummies?") The new fusing books which are on the market are a good thing to have (Petra Kaiser's is my personal fave) but they all pretty much cover the same basics. It would be good to offer people some new and easy avenues to explore to get their creative juices flowing.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

Lynn g
Posts: 91
Joined: Sun Nov 02, 2003 1:36 am
Location: Clovis, CA

Postby Lynn g » Mon Mar 22, 2004 1:06 am

Randy, this is so cool! Thank you! I have been curious about what I've read on the board about pot melts (and the maglesses I received) but haven't had time to hunt through the archives. Now you have saved me all that time and effort with a beautifully clear explanation. You should write a book!

I'm serious...maybe something along the lines of "Fun Things to Do with Your Kiln Without a Major Investment in Complicated Equipment". ("Fusing for Dummies?") The new fusing books which are on the market are a good thing to have (Petra Kaiser's is my personal fave) but they all pretty much cover the same basics. It would be good to offer people some new and easy avenues to explore to get their creative juices flowing.
Lynn g
"Patriotism is not enough, I must have no hatred or bitterness towards anyone." - Dame Edith Cavell

Barbara Silverberg
Posts: 19
Joined: Sun Dec 14, 2003 12:17 pm
Location: Cleveland, Ohio

Postby Barbara Silverberg » Mon Mar 22, 2004 8:21 am

Wonderful presentation! The pieces are beautiful and the explanation very clear. Thanks so much for sharing!

Randy W
Posts: 91
Joined: Sun Mar 09, 2003 6:19 pm
Location: Racine, Wisconsin

Postby Randy W » Mon Mar 22, 2004 9:17 am

You are all very welcome, and thanks for the compliments.
Please share a photo of some of your completed pot melts.

Randy
When injustice becomes law, rebellion becomes duty.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 38 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com