Armstrong & Youghiogheny Float Compatible glass

Post by quill »

I just got back from Glass Craft Expo. There was some great stuff. I got to take a lot of classes including a pate de verre class stack block class, a Bullseye box casting demo. Came back loaded to the gills with glass and tools & lots of great products.

I brought back some of Armstrong's new patterned & colored float compatible glass as well as Youghiogheny's colored transparent float compatible.

I have not done much with float but am hoping this glass will be fun.

Has anyone here tried it?
Dennis Brady
Posts: 64
Joined: Fri Dec 19, 2003 9:06 pm
Location: Victoria BC
Contact:

Post by Dennis Brady »

Haven't tried the Yucky but the Armstrong is terrific. Especially if you want to fire large pieces (like door lites). My ONLY complaint is there's so far a very restricted colour palette but I'm hoping that will soon be expanded. Having glass that can be fused onto large door lites and full size windows (6 to 8 ft tall) opens up many new opportunities for architectural applications.

Was that not a terrific show? When we were packing out after, there were people lined up to register early for classes next year. We've already booked a bigger exhibit booth and planning extra classes for 2005.
DeBrady Glass Ltd http://www.debrady.com
Victorian Art Glass http://www.vicartglass.com
Glass Campus online classes http://www.glasscampus.com
quill
Posts: 107
Joined: Wed Apr 02, 2003 10:35 am
Location: BC
Contact:

Post by quill »

Was that not a terrific show?
Well, I sure thought so! I will look for you next year for sure.
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Post by rosanna gusler »

so is this glass the same that is on their website? sort of a mottled enameled looking glass? rosanna
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Post by Bert Weiss »

rosanna gusler wrote:so is this glass the same that is on their website? sort of a mottled enameled looking glass? rosanna
Rosanna

I saw the Armstrong glass when I was in Portland. I was astounded at what garbage it was. It is enamel smeared on thin float glass. A total waste of glass and enamel to my eye. First of all, I often find thin and thicker float glasses incompatible. Second of all, The smeared enamels were ugly, poor imitations of stained glass.

I am curious about Yough's transparent colors. I wonder if they are more vibrant than Thompson's or lower melting temp than the CR LOO frits. I am more interested in the frits made from them than I am in using sheets. Thompson made wonderful colors before they took the lead out and killed the colors. Transparency is still an elusive factor for me with the exception of blue.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
quill
Posts: 107
Joined: Wed Apr 02, 2003 10:35 am
Location: BC
Contact:

Post by quill »

I saw the Armstrong glass when I was in Portland. I was astounded at what garbage it was. It is enamel smeared on thin float glass. A total waste of glass and enamel to my eye.
It is enamel on glass but I actually liked it. I am not sure it was meant tp look like stained glass, I think it has a distinct look that has lots of possibilities.

The Youghiogheny colors are really pretty. There is a Violet, a Kelly Green, a light blue & an Erbium Pink.
Lynne Chappell
Posts: 186
Joined: Fri Mar 14, 2003 2:05 am
Location: Surrey B.C. Canada
Contact:

Post by Lynne Chappell »

I was also disappointed with the Armstrong. I ordered a sample set, and was expecting real colored through the sheet glass, not an enamel coating.

Looking forward to seeing the Youghigheny glass.
watershed
Posts: 166
Joined: Wed Mar 12, 2003 1:44 am

Post by watershed »

Enamels on glass are "generally" more like Oil Paints, not like Stained glass. If you want that depth of color, get colored glass.

Youghigheny (sp) flat glass. Anyone have an address? I probably could/should search, but I'm typing right now. And the spelling would cause me much trial, even though , as a child, I went to Ohiopyle annually.

Greg
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Post by Brad Walker »

watershed wrote:Youghigheny (sp) flat glass. Anyone have an address?
Forgot the "o": http://www.youghioghenyglass.com/