Postby Glenda Kronke » Mon Apr 05, 2004 4:47 pm

I did the worst thing. I test fired some Ferro paints on float and forgot/didn't write down which tiles were which color :oops: I thought it would be fairly simple to tell which colors they were. Boy, was I wrong!

I made about a dozen 1" x 2" tiles of each of the following colors:

Red
Poppy
Manderine
orange

*also, lemon (very yellow), chestnut (dark brown) and ochre (tan)

(I fired to 1450/10 min)

Are the ugly 'brown' ones the red? (think dull brick red)
*should I have fired higher for the red?

Is Poppy really really bright reddish/orange
*these are really pretty!

Are orange and manderine really close? (these are the two that are confusing me the most)
One is lighter (more yellow?) the other is closer to poppy but still orange.
I know a manderine is an orange but is it darker than regular orange?

FYI/no comment needed... another no-no I did..... after I painted all the tiles, I had left over paint and painted some of the tiles by combining the left over paints - without writing down which paints I combined. Most of these are streaky so I know they are combos.

I will never do that (not take notes) again!

thanks,
g-

The Hobbyist
Posts: 302
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Postby The Hobbyist » Mon Apr 05, 2004 4:52 pm

If you are lazy like me another way to keep track, without all that writing, is to take before and after pictures of the layout on the shelf in/out of the kiln. Cheap too if you have a digital camera.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg

Stuart Clayman
Posts: 224
Joined: Mon Mar 31, 2003 12:35 pm
Location: Virginia
Contact:

Postby Stuart Clayman » Mon Apr 05, 2004 4:55 pm

since these are sample tiles something else to do is to write down the color with that paint. ie if lemon is on the brush, then write lemon..
Kiln Repair by a Clayman kilnrepair@yahoo.com
Glassworks by a Clayman
http://www.GlassArtists.org/GlassworksByAClayman

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Ferro paints/color

Postby Bert Weiss » Mon Apr 05, 2004 5:52 pm

Glenda Kronke wrote:I did the worst thing. I test fired some Ferro paints on float and forgot/didn't write down which tiles were which color :oops: I thought it would be fairly simple to tell which colors they were. Boy, was I wrong!

I made about a dozen 1" x 2" tiles of each of the following colors:

Red
Poppy
Manderine
orange

*also, lemon (very yellow), chestnut (dark brown) and ochre (tan)

(I fired to 1450/10 min)

Are the ugly 'brown' ones the red? (think dull brick red)
*should I have fired higher for the red?

Is Poppy really really bright reddish/orange
*these are really pretty!

Are orange and manderine really close? (these are the two that are confusing me the most)
One is lighter (more yellow?) the other is closer to poppy but still orange.
I know a manderine is an orange but is it darker than regular orange?

FYI/no comment needed... another no-no I did..... after I painted all the tiles, I had left over paint and painted some of the tiles by combining the left over paints - without writing down which paints I combined. Most of these are streaky so I know they are combos.

I will never do that (not take notes) again!

thanks,
g-


The ugly brown is probably a gold bearing red fired on the tin side. Poppy is a pretty dark deep red The other colors you should be able to pretty much tell the mandarin is a bit diffferent than the orange... The pale yellow is not the Mandarin.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Glenda Kronke
Posts: 64
Joined: Tue Mar 11, 2003 11:44 am
Location: Austin, TX
Contact:

Ferro paint

Postby Glenda Kronke » Mon Apr 05, 2004 6:15 pm

Bert,

Of the 3 'orange' colors I have; listed darkest to lightest

Poppy-darkest coloration (red/orange)

Manderine -medium coloration- orange

Orange- lightest coloration - orange

or should I reverse the last two?

I guess it isn't that important because I still have lots of tests to run and will run these colors again anyway. Was just curious and didn't want to wait another week to test.

Thanks,
glenda

ps will heed Stuart's and Jim's advice next time!

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Ferro paint

Postby Bert Weiss » Mon Apr 05, 2004 11:44 pm

Glenda Kronke wrote:Bert,

Of the 3 'orange' colors I have; listed darkest to lightest

Poppy-darkest coloration (red/orange)

Manderine -medium coloration- orange

Orange- lightest coloration - orange

or should I reverse the last two?

I guess it isn't that important because I still have lots of tests to run and will run these colors again anyway. Was just curious and didn't want to wait another week to test.

Thanks,
glenda

ps will heed Stuart's and Jim's advice next time!


Without looking, I think that is right.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 36 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron