LDGlass
Posts: 22
Joined: Sun Mar 23, 2003 2:54 pm
Location: Milwaukee, WI
Contact:

Glass Glue

Postby LDGlass » Mon Apr 05, 2004 10:47 pm

I have not been able to find the perfect way to bond a silver bail to the back of a fused glass pendant. Can someone suggest a type of glue or epoxy that works best for them? I have been using 2-part epoxy but I've noticed that it doesn't take too much force to separate it from the glass. Any suggestions are greatly appreciate. Thanks in advance! :lol:

Cher
Posts: 91
Joined: Tue Oct 07, 2003 8:59 pm
Location: MI
Contact:

Postby Cher » Mon Apr 05, 2004 11:01 pm

Don't know about perfect, but E6000 gets recommended a lot. Trick with that is to leave it alone for 24 hours. (sets quicker than that) silicone is also highly recommended. Good luck.
>^..^<

Paul Tarlow
Posts: 344
Joined: Sun Mar 09, 2003 4:06 pm
Location: Helios Kiln Glass Studio - Austin
Contact:

Re: Glass Glue

Postby Paul Tarlow » Mon Apr 05, 2004 11:33 pm

There are many, many threads on this in the archive.

You may want to start here:

http://www.warmglass.com/phpBB/viewtopic.php?t=829

- Paul

Laura Dawson wrote:I have not been able to find the perfect way to bond a silver bail to the back of a fused glass pendant. Can someone suggest a type of glue or epoxy that works best for them? I have been using 2-part epoxy but I've noticed that it doesn't take too much force to separate it from the glass. Any suggestions are greatly appreciate. Thanks in advance! :lol:

Claudia Whitten
Posts: 75
Joined: Sun Mar 09, 2003 9:32 pm
Location: Idaho
Contact:

Postby Claudia Whitten » Mon Apr 05, 2004 11:58 pm

Laura,
I had the same problem with pendants. I found that the earrings worked just fine with the 2 part epoxys. For the pendants I have changed to Dymax 621. I have been very pleased with it. I use an activator with it 535-A. I got my glue from Dewey Associates, 1-800-448-2306.
They will not come apart and they set up fast. I have to be careful to get them right the first time. Claudia
It's not the destination but the journey that feeds the soul.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 47 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com