Uroboros Fusion FX frit powder(90COE)...

Postby skin_mechanic » Thu Apr 08, 2004 11:24 pm

...I recently purchased the entire color palate. I'm kinda surprised at the inconsistancy of the texture among the various colors. Some colors are super fine(Grenadine Red), others are so coarse that they won't stay suspended in the mineral oil(Spearmint Green). Reading thru their catalog, the size of the powders range from .13mm to .25mm, but the granules look to be a lot larger than that. I'm wondering if some coarser grind got in to the mix somewhere. Contrary to what I had initially thought, the coarser powders are easier to paint with.

Bob
Posts: 215
Joined: Mon Mar 10, 2003 1:01 pm
Location: Salt Spring Island, British Columbia
Contact:

Postby Bob » Fri Apr 09, 2004 9:50 am

Dear Skin,

Those are my observations as well. BE powders are more consistent in grain size.

Cheers,

Bob


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 31 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com