Mother of Pearl Powders

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
nbaybear
Posts: 2
Joined: Thu Apr 08, 2004 6:51 pm

Mother of Pearl Powders

Post by nbaybear »

Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable


Thanks Randy :lol:
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Mother of Pearl Powders

Post by Brock »

nbaybear wrote:Has anyone used Mother of Pearl powders with either COE 96 or 90, would like to try but not sure if they are compatable


Thanks Randy :lol:
Compatability won't be a problem, but what is this stuff? If it's real nacre, it's just gonna burn up. Maybe they're another form of mica? Brock
My memory is so good, I can't remember the last time I forgot something . . .
Ron Coleman
Posts: 468
Joined: Sun Mar 09, 2003 3:20 pm
Location: Columbus, Ohio USA

Post by Ron Coleman »

If the Mother of Pearl powders are the ones from CR Loo, they will work.

Just another name for mica powders.