How fast to fire a pot melt

Postby Lonman » Sat Apr 10, 2004 8:48 pm

Can anybody please tell me how fast to get up to 1600+ degrees for a pot melt? Or does it even matter?

Thanks
Lonman 8)

Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Postby Steve Immerman » Sat Apr 10, 2004 9:51 pm

It only matters that if you go too fast it is theoretically possible that your pot or your shelf could crack. I usually use 2000dph.

Steve

revjerry
Posts: 28
Joined: Fri Dec 05, 2003 12:29 pm
Location: Coastal Maine
Contact:

Pot melt

Postby revjerry » Sun Apr 11, 2004 2:19 pm

Steve,
I'd like to see your kiln! Are you really able to make 1600 in less than an hour? Hate to have your electric bill. But that's a good answer. I know that my kiln doesn't go much faster than 900 an hour but I don't like going that fast. You know my process, and within that process I usually go at 600 an hour to protect the pots, kiln and the base glass. Probably faster won't hurt anything.

BTW, a customer was in the shop this week and asked if I'd ever considered making a pot melt into a table top? Interesting thought. Certainly there's size limits, but I think it can be done. Anyway, there's some new food for thought.

Will I see you in Corning?

Jerry

Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Re: Pot melt

Postby Steve Immerman » Sun Apr 11, 2004 5:05 pm

Revjerry wrote:Steve,
I'd like to see your kiln! Are you really able to make 1600 in less than an hour? Hate to have your electric bill. But that's a good answer. I know that my kiln doesn't go much faster than 900 an hour but I don't like going that fast. You know my process, and within that process I usually go at 600 an hour to protect the pots, kiln and the base glass. Probably faster won't hurt anything.

Will I see you in Corning?

Jerry


I have a Paragon GL22 with elements in the top, side and doors. I don't exactly know how fast it heats up when I set it to 2000dph. Never timed it. Next time, I'll keep an eye on the clock.

Not sure about Corning yet.

Steve

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Postby Brock » Sun Apr 11, 2004 5:10 pm

I'd like to see your kiln! Are you really able to make 1600 in less than an hour?

There's a certain engineer type on this board who has built the fastest kiln I've ever heard of.

Brock
My memory is so good, I can't remember the last time I forgot something . . .

Phil Hoppes
Posts: 297
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Postby Phil Hoppes » Tue Apr 13, 2004 8:33 pm

Hmm....now who would that be....

Can you say 3000 DPH!!

FireBoy

OBTW.....not the fastest. A prof at my old Alma Mater did a little better

http://www.discoverchemistry.com/dcv2-d ... fault.html

He got to 10,000 degrees in about 1/2 second. The faculty made him take down his web site. :-( I saw it before they made him remove it. VERY IMPRESSIVE!!!!

Havi
Posts: 587
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Postby Havi » Thu Apr 15, 2004 5:19 pm

:?

can you excuse me? what is pot melting? do you use a wok for this?? sorry to be such ignorant....... perhaps this is something new I could enjoy??

thanks,
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Cynthia

Postby Cynthia » Thu Apr 15, 2004 6:15 pm

heruviva wrote::?

can you excuse me? what is pot melting? do you use a wok for this?? sorry to be such ignorant....... perhaps this is something new I could enjoy??

thanks,


Havi,

There's a great book called Techniques of Kiln-formed Glass by Keith Cummings. In it he describes what he calls a 'kiln pour' and many variations on pouring... among many other techniques that we talk about on this board. If you want to learn many many different way to form glass in a kiln, this is THE book. Lots of information, history, great pictures...and more techniques than you can possibly ever even try.

A pot melt is simply a variant of pouring...Fill a clay flower pot with three colors of glass, divided into three sections, suspend the pot above the shelf with a bridge of kiln furniture and heat to about 1700F until it starts to flow out of the drainage hole and onto the shelf giving you a spiral design of how the glass flows onto the shelf (think honey off of a spoon...spin, drizzle).

Havi
Posts: 587
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Postby Havi » Fri Apr 16, 2004 12:27 am

Thank you guys for the pm's and the on board explanations!
I am very grateful! I remember now I tried this in one of the workshops I attended, it was not very successful, though

hopefully I shall try it again :D :D
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 65 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com