Postby MABeads » Tue Apr 13, 2004 8:17 pm

:roll: Hi all,
I have not been on for a long time and I was trying to search the archives for an answer but they are not that current.
I want to make something in burgundy using dichroic. Just a pendant size piece. Has anyone figured out a good comb of dichro and a flash color to make burgundy?
Thanks,
Mary Anne

GlassOrchid
Posts: 57
Joined: Wed Apr 16, 2003 9:35 pm
Location: Maine
Contact:

dichro color

Postby GlassOrchid » Tue Apr 13, 2004 10:42 pm

that's a tough one..... the closest color I can think of in art glass would be cranberry or deep plum (1311 or 1105) but for dichro it's difficult. Perhaps black cherry on clear on one of the art glasses above? There really is no dichro that color but if you play with a combo of art glass and dichro on clear you might be able to hit something close to what you want...

Luck,
Nancy

Kitty
Posts: 437
Joined: Sun Mar 09, 2003 4:12 pm
Location: Gig Harbor, WA

Postby Kitty » Tue Apr 13, 2004 11:05 pm

i agree with nancy. whatever "burgundy" means, that range is achieved with cranberry as a base, and sometimes with BE gold/purple as the base, then one of these CBS colors, on clear: dark dark red, black cherry, or dark red. if you put a little overlay of neo-lavender on top, it will be a little more of a wine color. red earrings didnt sell for years, but now they do, which is how i happen to know about these combinations. i make everything out of thin glass, and within the word "thin," i get the thinnest sheets available. makes for better blended colors, and less weight. maybe you can buy a sample square of black cherry from CBS and try it on different base colors, see what u think.

MABeads
Posts: 2
Joined: Sat Jan 31, 2004 7:36 pm

Postby MABeads » Wed Apr 14, 2004 12:32 am

I have a piece of black cherry CBS dichro on black. I am trying it with neo lav. on top right now. If I get a wine color that is fine. Had not thought of the clear black cherry, that is a good suggestion. Maybe even on a deep rose opaque, or maybe one of the blues. Burgundy is a bluer shade of red so it might work.

Thanks for the suggestions.
Mary Anne

KatyPattison
Posts: 21
Joined: Sun Mar 09, 2003 4:51 pm
Location: Canada
Contact:

Postby KatyPattison » Wed Apr 14, 2004 9:46 am

CBS rainbow (I think premium) has one section in it that might be considered "burgundy". Finding the exact section could be tricky though!

Katy


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 62 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron