Page 1 of 1
Stiff Black
Posted: Thu Apr 15, 2004 11:01 pm
by Amy on Salt Spring
Just got my BE catalog today (finally). After going through it about 10 times I was actually able to settle down and really look at everything. Since I have a fondness for black and white pieces I was very interested in the new Stiff Black available. I'm wondering if anyone has used it yet and if so what they thought of it. They say its not as soft as regular black--I'm wondering what it does at different temps and is it more resistant to kiln wash sticking than the regular black? Any info. would be greatly appreciated.
Amy
Posted: Fri Apr 16, 2004 1:04 am
by gone
I think it will be nice for textured pieces (in the kiln) and for a satin finish when used with other colors. I don't care for the way the black is always a little shinier.
Posted: Fri Apr 16, 2004 8:26 am
by Marty
It doesn't bleed like the soft black, viscosity is closer to the opals, so you'll get a crisper edge between the colors. It's nice to have another tool in the box.
Posted: Fri Apr 16, 2004 11:06 am
by Amy on Salt Spring
I'm getting the impression its only for pieces that are full fused--not for anything sintered or in between sintering and full fuse. I mean at what temp. does its edges soften? If the only benefit is that it doesn't bleed--that isn't an issue in anything less than full fuse.
-A
P.S.Why will it be less shiny Els?
Posted: Fri Apr 16, 2004 11:19 am
by Jackie Beckman
It will be less shiney because:
If you've fused and sandblasted and want to keep a matte finish during a low firepolish or slump, you may fire to 1150. Els is saying that when the rest of the glass is where she wants it, the black begins to shine up again.