Postby Jackie Beckman » Fri Apr 16, 2004 11:57 am

I've tried three times to respond to your email question, but it keeps bouncing back. :-k

When you said "tile" I thought you meant tile, like backsplash tile. So disreguard the advise I gave you if you were asking about Joseph's Pride. That piece has nine panels, each with a different texture. Which one are you referring to?

Jackie

slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

jp

Postby slats » Fri Apr 16, 2004 2:30 pm

dont have them to refer to but.......curious how the patterns were acheived.no one in particular..........s.andblasted?

Jackie Beckman
Posts: 475
Joined: Sun Mar 09, 2003 5:01 pm
Location: Arizona
Contact:

Postby Jackie Beckman » Fri Apr 16, 2004 3:20 pm

Everything I make gets sandblasted as the first step. From there, depending on the particular surface I want, I either hand polish, carve, polish with discs, or a combo of all of those. If there is a certain look you saw someplace that you like or want to know more about, feel free to specify and I'll try to be more clear.

Jackie


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 54 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com