Post by Tamara Baskin »

I would like suggestions as to the correct equipment used to polish the bottom dull side of fused bowls coming out of the kiln.
Tamara baskin
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: polishing

Post by Brock »

Tamara Baskin wrote:I would like suggestions as to the correct equipment used to polish the bottom dull side of fused bowls coming out of the kiln.
Tamara baskin
It's very difficult, and time consuming, to polish a large curved surface like that. I suggest you sand blast the bottom of your blank prior to firing. This will give you a dull sheen on the bottom, after slumping, that is more resistant to marks and fingerprints than unfired sandblasting. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: polishing

Post by Bert Weiss »

Tamara Baskin wrote:I would like suggestions as to the correct equipment used to polish the bottom dull side of fused bowls coming out of the kiln.
Tamara baskin
The only solution I know if is to do a drop slump through an empty hole, cut off the overhang (small glass cutter or very large diamond saw), grind it flat on a lap wheel and polish it out on two or three vibralaps. Many thousands of dollars later, you can do it. See the work of Stephen Schlanser. He sometimes blasts patterns to avoid some polishing or cover blemishes.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
susan fancy
Posts: 4
Joined: Thu Apr 03, 2003 6:27 pm
Location: Ann Arbor, Michigan

Post by susan fancy »

A duller back surface is characteristic of fused work. If you're interested in "glossy on 2 sides" work, glassblowing is a better technique.
Steve Immerman
Posts: 208
Joined: Sun Mar 09, 2003 4:55 pm
Location: Eau Claire, Wisconsin
Contact:

Post by Steve Immerman »

Using Bullseye iridized glass with the irid side down, on a nice, smooth, kilnwashed shelf gives a nice bottom.

Steve
Dick Ditore
Posts: 58
Joined: Mon Mar 10, 2003 12:56 pm
Location: San Diego, Ca
Contact:

Post by Dick Ditore »

You can use a flat lap and grind the blank and polish before you slump.

Dick