SONYA
Posts: 5
Joined: Tue Oct 07, 2003 12:36 pm
Location: Scotland

Fusing glue

Postby SONYA » Mon Apr 19, 2004 9:46 am

I'm interested in information about fusing glue. Must you always use specially formulated fusing glue or are there other products or normal household things you can use which would just as effective?

Phil Hoppes
Posts: 297
Joined: Wed Mar 12, 2003 2:20 pm
Location: Overgaard, AZ

Postby Phil Hoppes » Mon Apr 19, 2004 9:52 am

Elmers glue - dilute it 50% with water. Works fine.

Andrew
Posts: 46
Joined: Fri Apr 11, 2003 1:39 pm
Location: Minnesota
Contact:

Be careful how you use it

Postby Andrew » Mon Apr 19, 2004 10:01 am

Dilute Elmers at least 50%. The manufacturers claim that the glue burns off and leaves no residue but I haven't found this to be true. Glue on the surface usually burns off completely, but I have seen residue when the glue is trapped between layers - especially between clear. Just be careful how and where you use it.

SONYA
Posts: 5
Joined: Tue Oct 07, 2003 12:36 pm
Location: Scotland

fusing glue

Postby SONYA » Mon Apr 19, 2004 10:34 am

I don't think you can get Elmers glue in Scotland(UK) so can anyone in Britain help me out with fusing glue?

Brad Walker
Site Admin
Posts: 1374
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: fusing glue

Postby Brad Walker » Mon Apr 19, 2004 10:49 am

SONYA wrote:I don't think you can get Elmers glue in Scotland(UK) so can anyone in Britain help me out with fusing glue?


Elmer's glue is a brand name for white glue. This is from a family of glues called PVA glues. PVA stands for poly vinyl acetate.

You can find it in the UK in children's stores (such as Early Learning Centre) or in DIY stores (it's used for stabilising plaster prior to wallpapering). PVA is probably the most widely used glue in the world, so other places will certainly have it also.

The key to using glues with glass is to dilute the glue and use as little as possible. And remember, the glue burns off at around 900F/480C -- it doesn't hold the glass until it fuses, just holds it to help you get it in the kiln.

SONYA
Posts: 5
Joined: Tue Oct 07, 2003 12:36 pm
Location: Scotland

fusing glue

Postby SONYA » Mon Apr 19, 2004 12:52 pm

Thank you so much Brad Walker for your reply. I'll now be able be go out and buy some. I imagine it will be cheaper than buying dedicated fusers glue.

Bert Weiss
Posts: 2338
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Postby Bert Weiss » Mon Apr 19, 2004 1:14 pm

I've been messing around with CMC. It is a powdered binder that is mixed in hot water until diluted and then can be thinned to whatever consistency is desired. I put in a pot of water that has boiled and cooled a bit then stirred until it is all diluted. This can then be thinned with cold water.

In high concentrations, CMC serves to keep solids suspended in a liquid. the threads of the methyl cellulose hold particles in suspension.

I believe that Klyr Fire is a weak concentration of CMC. At some point you can coat frits with a water/CMC solution and when it dries it will be stuck. The binder in the CMC burns off cleanly and will also do so when used between layers of glass.

I'm pretty sure this works on the finer frits, I'm not sure how heavy a frit it will hold.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Anea
Posts: 41
Joined: Fri Mar 14, 2003 9:20 pm
Location: Monterey CA
Contact:

Postby Anea » Mon Apr 19, 2004 2:33 pm

I have been an avid user of Klyr Fire for over two years. It works great between layers and holds stringer and frit well, but not well enough to be turned upside down, until dry. If you want to be able to flip it upside down, sort of like a tack fuse without the fusing, try Krazy Glue. It works wonderfully well. Patty Gray taught me that, and she has also experimented with other brands, and said that she gets the most consistent results with the Krazy Glue brand. I personally haven't tried any other brands due to her advice, but have been using the Krazy Glue for a while with no burn out, residue, or other problems.

Anea

Susan Robinson
Posts: 5
Joined: Tue Apr 13, 2004 1:45 pm
Location: New Mexico
Contact:

follow up question

Postby Susan Robinson » Mon Apr 19, 2004 2:35 pm

Andrew wrote:Dilute Elmers at least 50%. The manufacturers claim that the glue burns off and leaves no residue but I haven't found this to be true. Glue on the surface usually burns off completely, but I have seen residue when the glue is trapped between layers - especially between clear. Just be careful how and where you use it.


I've been using diluted elmer's and find this, too. Works fine for opaque and dark pieces, but I'm making dichroic jewelry and find sometimes it leaves a smudge or flaw on the dichroic surface. Is this a place to use fuser's glue? (that is, does special fuser's glue *not* leave a smudge on clear dichroic?) I've been trying not to use glue now on clear pieces, but when putting lots of little pieces on a shelf it's a zen test a little above me, and I find myself snarling at the cats if they come too close to the work table...

-Susan

Rebecca M.
Posts: 126
Joined: Fri Sep 12, 2003 12:15 pm
Location: Myrtle Beach
Contact:

Postby Rebecca M. » Mon Apr 19, 2004 3:20 pm

I've been using Aileen's Tacky glue. Clear, dichro, whatever and it hasn't left a mark. Sets up pretty fast too. I don't water it down either, just a little dab with a toothpick. I don't much like any Elmer's products, that's just personal preference I guess.
Didn't Tony Serviente do a bunch of different glue tests and post the results? I think it was him.

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Postby Lauri Levanto » Mon Apr 19, 2004 3:30 pm

Like Bert, I have used CMC. For those who are afraid of chemical terms, I can tell it is the stuff that makes jam to a jelly and not juice.

I had a class at Päivi Kekäläinen ( for Englsh speaking friends Paevi Kekaelaeinen). She used starch as a binder in
thin pate de verre. CMC is very close to starch.

Dries slowly, does not hold until almost dry.

For quickies I use 5 sec. Cyanoacrylate.
-lauri

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

P.s.

Postby Lauri Levanto » Mon Apr 19, 2004 3:32 pm

I add some CMC into kilnwash, too.
It gives harder surface that I can sand smooth.
-lauri

dan
Posts: 6
Joined: Mon Mar 10, 2003 3:43 pm
Location: Lincoln, England
Contact:

Postby dan » Mon Apr 19, 2004 4:03 pm

u can get elmers glue from creative glass in kent..pearsons also sell a type of fusing glue,i use the 1 in liverpool but think theres also 1 in east kilbride theyll send it out anyway....ive been using super glue for the past few months + its working fine,no residue or nowt... dan.
dan.

SONYA
Posts: 5
Joined: Tue Oct 07, 2003 12:36 pm
Location: Scotland

Fusing glue

Postby SONYA » Mon Apr 19, 2004 6:40 pm

Thanks alot everyone. This is my first time using the Bulletin Board and I'm so impressed with the response. Dan you say you use Super Glue. Do you use this to stick glass together prior to fusing?

Valerie
Posts: 42
Joined: Sun Mar 09, 2003 7:01 pm
Location: Kentwood Michigan

Postby Valerie » Mon Apr 19, 2004 8:58 pm

Clear nail polish works in pinch for me also

Tony Serviente
Posts: 328
Joined: Thu May 29, 2003 11:48 am
Location: Ithaca,NY
Contact:

Postby Tony Serviente » Mon Apr 19, 2004 9:13 pm

I glue up alot of things that either have to be moved into a kiln from across the room, are too difficult to lay up on a kiln shelf or need to flipped and fired face down. White glue has all the attributes I need. It can handle non flat, and even heavily textured glass. It sets up within an hour. It has a flexible bond that allows for easily handling of the glued up pieces. It is cheap, easy to obtain and is non toxic. I use it full strength, sparingly, and only along the edges. It can be very capricious, sometimes leaving no trace and sometimes a lovely black spot, but kept along the edges almost always gives a clean burn off.


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 63 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron