Postby Valerie » Tue Mar 11, 2003 10:40 pm

I have taken my 90 coe scrap and cut it up in very small pieces with the mosaic cutters and I would like to put it in a shallow bique plate mold. If I ramp up very slowly with a hold time at 1250/1300 could this work?
I have washed and air dried my scrap, and kiln washed my mold.
Thanks in advance for any and all advice Valerie

Barbara Muth
Posts: 382
Joined: Sun Mar 09, 2003 8:10 pm
Location: Washington DC Metropolitan Area
Contact:

Postby Barbara Muth » Tue Mar 11, 2003 10:58 pm

Valerie, you need to fuse the scraps together before you slump.

Barbara
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Valerie
Posts: 42
Joined: Sun Mar 09, 2003 7:01 pm
Location: Kentwood Michigan

Postby Valerie » Tue Mar 11, 2003 11:16 pm

I guess I was not clear on what I wanted ...I want to fuse the scraps in the bisque mold ...like a casting? Is that the correct term?
I did not have very good luck with fiber board so I thought I could use the bisque plate mold to "fuse" my scraps in

Brad Walker
Site Admin
Posts: 1286
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Postby Brad Walker » Tue Mar 11, 2003 11:29 pm

If you want your scraps to fuse together in the bottom of your mold, then you will need to fire higher than 1250/1300 F. Try around 1450/1500 F (800C). This should work, but make sure you have a good coat of kiln wash on your mold.

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Postby Lauri Levanto » Wed Mar 12, 2003 4:33 am

I do almost all my work in frit casting in bisquit mold.
MOst pieces are shallow reliefs, essentially flat.

As Brad said some 800-840 C is a proper temperature,
but ramp up slowly at two stages

570-600 C, the quarz inversion point at 573 C is quite a stress for a large flat mold.

650-700 C spend at least one hour to prevent the trapped air
to form bulges below the melted surface.

lauri
P.s. I kilnwash my molds before bisquit firing, so the 1st
layer of kilnwash is absorbed by the clay.

In subsequent firings in these temps you need a new
coat of kilnwash

Valerie
Posts: 42
Joined: Sun Mar 09, 2003 7:01 pm
Location: Kentwood Michigan

Postby Valerie » Wed Mar 12, 2003 7:47 am

Thanks everyone for their input. I knew I had to go slow from my previous attempt. I just thought holding longer at a lower temp would take the stress off the mold. I will put an extra layer of wash on before attempting this. :idea:


Post Reply

Return to “Techniques and Tools”

Who is online

Users browsing this forum: No registered users and 12 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com