devit on my yellow bullseye glass plates????

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
deborahbur
Posts: 51
Joined: Thu Apr 10, 2003 2:09 pm
Location: Tiverton, Rhode Island
Contact:

devit on my yellow bullseye glass plates????

Post by deborahbur »

I am having problems with my yellow glass ( I am also using light blue,lavender and light green) getting cloudy when I fuse and slump.

Is there more of a problem with yellow? Should I be using something on the yellow? HELP> Sometimes the yellow is clear, but mostly a little cloudy.

I fuse 3 or 4 shelves and slump the same in a skutt kiln. I fuse to 1490 and slump to 1300. Any ideas?

Once, I put the yellow glass on the bottom shelf and it came out really clear, but another time I did the same thing and it came out cloudy.