Not crying but................
Posted: Thu May 15, 2003 11:53 am
Yesterday morning I thought I would be crying because the kiln did not shut off and the kids tiles cooked at 1300 for over 14+ hours.
I have learnt my lesson and will start the kiln in the AM. This way I will know that it is on the cool down by the time I leave school.
Here is a link to the glass art page if the school website.
The first 2 pics are of the good tiles, 2nd two pics are of the tiles from when the kiln did not shut off correctly.
The last pic is of some pins I made teachers.
I have at least 4 more batches of tiles to fuse. The kids have had a great time doing them.
http://www.anoka.k12.mn.us/education/co ... 1053013510
I have learnt my lesson and will start the kiln in the AM. This way I will know that it is on the cool down by the time I leave school.
Here is a link to the glass art page if the school website.
The first 2 pics are of the good tiles, 2nd two pics are of the tiles from when the kiln did not shut off correctly.
The last pic is of some pins I made teachers.
I have at least 4 more batches of tiles to fuse. The kids have had a great time doing them.
http://www.anoka.k12.mn.us/education/co ... 1053013510