weird haze Q

Post by rodney »

i was playing around, and put in some glass strips to fuse ,,,what i did was cut the glass, wash it with water, put in in the kiln wet, fire it, and then when it came out, it had this haze sort of thing on it, very vague, but not good,,im wonderin if the glass being wet is resonsible, or if the water i put on it when it came out, and still hot made it,,,or if it is something totally different,,,would using a borax spray prevent such a thing, from happening, or would borax solve the problem if i cut it up and refused

as always, thanks for all the info

rodney