Ideas for Breaking Bottles
Moderator: Tony Smith
Ideas for Breaking Bottles
I am trying to break wine bottles to get large chunks of glass to do some fusing. I have recently tried to wrap the bottle in a plastic bag, and strike it with a hammer. The result more shattering, with a lot of small pieces, and very few large pieces.
Any ideas of how I can break these bottles and get larger pieces of glass?
Any ideas of how I can break these bottles and get larger pieces of glass?
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Ideas for Breaking Bottles
Looking at your website, it appears you must be using a tile saw to cut bottles. Can't you just chop them up in bigger sizes with your saw?
Re: Ideas for Breaking Bottles
I could, but that is a bit time consuming, plus I am looking for more of a "broken" look.Valerie Adams wrote:Looking at your website, it appears you must be using a tile saw to cut bottles. Can't you just chop them up in bigger sizes with your saw?
Re: Ideas for Breaking Bottles
Score. Tap. Break . . .
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Ideas for Breaking Bottles
Would it work tomheat it in the kiln then dunk into a bucket of cold water?? Never tried it but might be interesting.........
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: Ideas for Breaking Bottles
As Brock said. Make a few random scores on the clean bottle, then stick it in your plastic bag and whack it with the hammer. It'll still break, but the scores will relieve some of the shattering.
You could also try dropping it on a corner of a concrete stair from about 3 feet up. When I do that the bottle always breaks, and there goes the wine...
You could also try dropping it on a corner of a concrete stair from about 3 feet up. When I do that the bottle always breaks, and there goes the wine...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Tom Fuhrman
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: Ideas for Breaking Bottles
also try scoring and then put in a box and hit it with a sharp flame from a torch. It should give you nice larger pieces.
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Ideas for Breaking Bottles
That' how I do it.Tom Fuhrman wrote:also try scoring and then put in a box and hit it with a sharp flame from a torch. It should give you nice larger pieces.
Bob
-
Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: Ideas for Breaking Bottles
Hitting it with a hammer is applying too much force.
Try putting it in a plastic bag, tying a knot in the plastic bag, and dropping it from a moderate height onto a hard surface eg stand on a chair and drop it on it's side onto concrete.
Try putting it in a plastic bag, tying a knot in the plastic bag, and dropping it from a moderate height onto a hard surface eg stand on a chair and drop it on it's side onto concrete.
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Ideas for Breaking Bottles
"Hitting it with a hammer is applying too much force."
That might just depend how hard you hit it, doncha think?
That might just depend how hard you hit it, doncha think?
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Ideas for Breaking Bottles
Isn't doncha think the sound of a correctly scored and struck bottle breaking? 
-
Tammy Macdonald
- Posts: 15
- Joined: Tue Jun 18, 2013 1:45 pm
- Location: Texas
Re: Ideas for Breaking Bottles
I'd guess the correct spelling would be -- doncha TINKKevin Midgley wrote:Isn't doncha think the sound of a correctly scored and struck bottle breaking?
Re: Ideas for Breaking Bottles
For fun & in the name of science, you could also try lighting up your propane torch and hit the bottle with the flame...
Maybe fry it in a pan like we used to do with marbles?
Maybe fry it in a pan like we used to do with marbles?
please visit Beall Glass Studio on Face Book