Postby barclayb » Sun Aug 31, 2014 12:51 am

Someone has probably either thought of these things & posted or has a reason not to do them :)


After trying glass cleaner and alcohol to clean glass, I had an "aha" moment and started using vinegar. (I think someone here suggested soaking glass in it to get the kiln wash out; one thing led to another ...) It works great! Duh, it's what people rinse crystal in to make it pretty and de-smudged.


There are sometimes a few stubborn little divits of kiln wash on the underside of a flat piece; I've been using a dental pick to chip the kiln wash out (especially if I'm going to slump anyway).


To stop having to measure a mold every time I use it (my memory being like a sponge that's been wrung out), I've started using Glassline paint to mark the size on it. Once the mold is fired, the markings seem to be permanent. [Am I wrong about that?]
from the whimsical and peripatetic world of
Barclay Elizabeth Blanchard
(pronounced Barkley)
servant of cats

David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: ideas: cleaning glass & marking molds

Postby David Jenkins » Sun Aug 31, 2014 11:05 am

Good start to a "Glass Hacks" thread - thanks!
Dave Jenkins
Glass at Harbor Gates
Cypress, TX

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: ideas: cleaning glass & marking molds

Postby Laurie Spray » Sun Aug 31, 2014 6:07 pm

I like to mark my molds also. I do it with a ceramic pencil (does not burn off) under the lip. I position them on the shelf so that I can read the size without picking them up. I stack my mold gently so this saves alot of time.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Ed Cantarella
Posts: 146
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: ideas: cleaning glass & marking molds

Postby Ed Cantarella » Tue May 08, 2018 9:41 am

Glassline paints,etc. - mark the weight of fill on all casting molds. :wink:
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron