Hello ! Is it possible to do a potmelt with only transparant glass colours ? I did try it once.....all colours became dark ? Thank you ! Jan

DonMcClennen
Posts: 345
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Potmelt from transparent glass

Postby DonMcClennen » Sun Aug 26, 2018 4:21 pm

You will need to have your pot filled with at least 50% clear plus stick with lighter shades of transparent glass!
"The Glassman"

JestersBaubles
Posts: 670
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Potmelt from transparent glass

Postby JestersBaubles » Thu Aug 30, 2018 9:54 pm

Avoid reds, and pay attention to not mix reactive colors (or at least separate them from each other with a layer of clear).

Dana

Jan de Jong
Posts: 74
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Potmelt from transparent glass

Postby Jan de Jong » Mon Sep 03, 2018 8:00 am

Thank you both for your answer ! I will try again. Jan de Jong

Sharol
Posts: 99
Joined: Sun Mar 05, 2006 2:45 pm
Location: Paradise, CA

Re: Potmelt from transparent glass

Postby Sharol » Fri Sep 07, 2018 10:57 pm

In addition to reds...orange and yellow transparents will have a tendency to opalize at pot melt temperatures. So, unless you’d like this effect, you should avoid these colors.

Sharol

Jan de Jong
Posts: 74
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Potmelt from transparent glass

Postby Jan de Jong » Sat Sep 15, 2018 4:56 am

Thank you Sharol ! Jan


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com