Hello ! Sorry, I forgot the recipe for this product to make "glue". Thank you, Jan de Jong

Jan de Jong
Posts: 78
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Carboxymethylcellulose (CMC)

Postby Jan de Jong » Sun Apr 14, 2019 5:04 am

Hello, Please give me an idea about how many (tea)-spoons on how many water I have to boil . Thank you very much !!! Jan de Jong (from Holland)

Barry Kaiser
Posts: 261
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Carboxymethylcellulose (CMC)

Postby Barry Kaiser » Mon Apr 15, 2019 9:53 am

There are a lot of different CMCs. In general use 3-4 tablespoons to a pint of hot water for a nice viscous solution.
That is good to hold powder together.
Your definition of "glue" also makes a difference. It depends on what you want to accomplish

Kevin Midgley
Posts: 633
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Carboxymethylcellulose (CMC)

Postby Kevin Midgley » Mon Apr 15, 2019 8:02 pm

However you may find that less is more than that suggested by Barry. The less you use, the less there is to burn out in the kiln and to not leave residues.
It will depend on the CMC you buy and how much glue power you need to use.

Jan de Jong
Posts: 78
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Carboxymethylcellulose (CMC)

Postby Jan de Jong » Tue Apr 16, 2019 11:22 am

Thank you both ...Barry and Kevin !!! Now I have an idea and I will test. Jan de Jong (from Holland)

Barry Kaiser
Posts: 261
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Carboxymethylcellulose (CMC)

Postby Barry Kaiser » Thu Apr 18, 2019 1:07 pm

When firing, vent the kiln to 1000 F and hold at that temp for about 10-15 minutes. That burns off all the organics.

Jan de Jong
Posts: 78
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Carboxymethylcellulose (CMC)

Postby Jan de Jong » Mon Apr 22, 2019 10:36 am

Hello, Giving birthday - ( to youth) and other workshops not at my home I need "glue" to attach pieces of glass on a blank glass (underground) ….for the transport. I tested the CMC I have: 3 TEA-spoons CMC on 1 liter water. Boiled and cooled it...and there was a solution, what was not like water....somewhat thicker. I tested it and it did his work good , but not so quickly !! But the solution (without the full gluing) hold the two parts of glass together ! I did fire to 780 C. (without venting) and no residuSorry …..my explanation is poor...due to my bad knowledge of the English language. I hope you will understand what I try to let you know, Jan de Jong (from Holland)


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 4 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com