Kiln element compatibility with stainless?
Moderator: Tony Smith
- 
				Mike Garvey
- Posts: 6
- Joined: Wed Jan 15, 2020 11:26 am
Kiln element compatibility with stainless?
I am thinking to add a small stainless washer to a kiln element (Kanthal) tail as it passes out of the kiln in order to prevent the tail from cutting into the soft firebrick.  Can I use stainless or do I have to go the ceramic route?  Thanks....Mike
			
			
									
						
										
						Re: Kiln element compatibility with stainless?
Either will work.  I used ss fender washers.
			
			
									
						
										
						- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Kiln element compatibility with stainless?
Ceramic tubes are available.   Old knob and tube wiring tubes could work as well.   Get your wiring inspected before using.