I just glued a batch of COE 90 frit balls to flat 6mm Christmas trees made from COE 96 glass. Oops. Does anyone know I might be able to get away with firing these? The dark shadows are gold decals I intended to fire to 1350 for 11 minutes, with the frit balls.
Thank you.
COE 90 frit balls ok on COE 96 Christmas trees?
Moderator: Tony Smith
-
Michael Stevens
- Posts: 83
- Joined: Thu Dec 26, 2019 2:52 pm
Re: COE 90 frit balls ok on COE 96 Christmas trees?
you might be able to tack fuse, but really it could crack later. personally, I'd make compatible frit bslls
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: COE 90 frit balls ok on COE 96 Christmas trees?
I use a little bit of my paints....just a dot, to attach the balls. This seems to act as a buffer for the differing COEs.
Remember the contact area is very small.
Remember the contact area is very small.
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns