BE opaline strike temp - WarmGlass.com

BE opaline strike temp

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
jim simmons
Posts: 459
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

BE opaline strike temp

Postby jim simmons » Sat Nov 14, 2020 6:57 pm

I have some BE Opaline striker and need to know what temp to take it to so that it strikes.
Thanks
The other Jim

Jan de Jong
Posts: 105
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: BE opaline strike temp

Postby Jan de Jong » Mon Nov 23, 2020 1:40 pm

Jim, no answers so I decided to try to help you but I am not sure you mean this! Bullseye site: Opaline striker....Full fuse. Jan