Postby Barbara Muth » Tue Dec 25, 2007 5:24 pm

I have been able to get a reduction atmosphere in my kiln without burning anything more than the organics many people use routinely in their kilns. While I never tried the reduction frits, I silver fume glass all of the time.
There are only three glasses in this piece - black, vanilla, and gray. The gradation of coloring is the result of silver fuming. There is some fading on subsequent firings, unless if you cap the fumed glass.

Image
Barbara
Check out the glass manufacturer's recommended firing schedules...
LATEST GLASS

Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron