My kiln is 11" deep, with top and side heating elements. I have a 7" high flower former I would like to use. Allowing for kiln shelf and 1" posts, does this leave the glass too close to the heating element? This is probably an elementary question but have just purchased this kiln and am still at the "know nothing" stage.

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Flower former too high for kiln?

Postby Valerie Adams » Fri Jun 15, 2012 9:34 pm

Take out the kiln shelf and place the flower former on the bottom of the kiln. Fire slow.

Pat Reynolds
Posts: 6
Joined: Mon May 28, 2012 12:23 am

Re: Flower former too high for kiln?

Postby Pat Reynolds » Sat Jun 16, 2012 4:32 am

Thank you, Valerie. Great idea.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Flower former too high for kiln?

Postby bob proulx » Sat Jun 16, 2012 6:21 am

Make sure your kiln floor is well kiln washed.
Bob


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 1 guest

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com