Postby Franzeska » Sat Sep 22, 2012 4:28 pm

Ceramaguard for molds and dams? The Armstrong website has a long list of tiles? Fine fissured, School Zone, Health Zone, Ultima, on and on. Which one?

Thanks.

Franzeska

Barb R
Posts: 58
Joined: Tue Jul 26, 2005 3:02 pm
Location: Ft. Collins, CO

Re: Ceramaguard

Postby Barb R » Sat Sep 22, 2012 8:31 pm

Maybe this will help..


http://www.warmtips.com/20050910.htm

Barb

CH Glass
Posts: 14
Joined: Sun Mar 21, 2010 3:43 pm

Re: Ceramaguard

Postby CH Glass » Sat Sep 22, 2012 8:41 pm

I've also tried to find Ceramaguard tiles. I've looked at Lowes and Home Depot, and found ceiling tiles made by Armstrong, but they do not specifically say Ceramaguard. I plan to try a commercial builders supply next. Any other suggestions?

Franzeska
Posts: 61
Joined: Tue Jul 24, 2012 10:46 am

Re: Ceramaguard

Postby Franzeska » Sat Sep 22, 2012 9:21 pm

Got it. Thanks.

Brad Walker
Site Admin
Posts: 1355
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Ceramaguard

Postby Brad Walker » Sat Sep 22, 2012 11:59 pm

CH Glass wrote:I've also tried to find Ceramaguard tiles. I've looked at Lowes and Home Depot, and found ceiling tiles made by Armstrong, but they do not specifically say Ceramaguard. I plan to try a commercial builders supply next. Any other suggestions?


You can't buy Ceramaguard at Lowes or Home Depot, only a commercial builder's supply place.

They'll generally make you buy a full case of the tile. If you want less than that, we sell it by the square foot at www.warmglass.org

CH Glass
Posts: 14
Joined: Sun Mar 21, 2010 3:43 pm

Re: Ceramaguard

Postby CH Glass » Sun Sep 23, 2012 3:17 pm

Thanks, Brad!


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 8 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com