Postby tgotch » Sat Dec 29, 2012 3:25 pm

I bought my first kiln from Paragon. The kiln arrived shortly before the holiday. They included the shelf, but unfortunately there were no legs in the shipment. They are closed for the holiday, and I am eager to do some playing around :twisted: I probably won't get the posts from them for over a week.

I am planning on slumping some bottles, and have some molds.

My question is: Can I lay the shelf flat on the bottom of the kiln (without the legs), and place the mold on the shelf, to do some test firing/slumping? Or should I just wait until the shelf posts arrive? I know this won't give me a true representation of firing schedules, but I want to play around a little, and make sure I don't mess up...

Thanks.

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln Shelf Question

Postby Kevin Midgley » Sat Dec 29, 2012 3:29 pm

yes

tgotch
Posts: 36
Joined: Mon Nov 14, 2011 11:04 pm

Re: Kiln Shelf Question

Postby tgotch » Sat Dec 29, 2012 3:34 pm

Thanks for the quick reply Kevin...to clarify...yes I can place the shelf directly on the floor?, or yes I should wait for the posts? :D

Any caveats?

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Kiln Shelf Question

Postby Laurie Spray » Sat Dec 29, 2012 4:21 pm

You can do it....just add a little time to the anneal stage
patience is one of the hardest lessons in glass work! :)
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln Shelf Question

Postby Kevin Midgley » Sat Dec 29, 2012 6:04 pm

rolling !!!! #-o :-k


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 11 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com