Hi,
I have a paragon glass kiln with heating elements in the lid. I started slumping bottles, and am concerned about bottles rolling into the walls while firing. I put a small piece of thinfire under the sides, but still worry about rolling.

Can I put kiln wash on the walls in case the bottles were to come in contact with them? I was reading Paragon's FAQ which states do not put kiln wash on walls, but it appears this may be referring to a kiln with elements in the walls.

Thoughts?

S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Kiln Wash on Walls

Postby S.TImmerman » Thu Jan 17, 2013 3:45 am

Is your kiln level? I have never slumped a bottle however i doubt they would roll around that much. You could put a barrier up made of kiln posts or thinly cut kiln shelves. Even cut up bottle rings would work.
Good luck

tgotch
Posts: 36
Joined: Mon Nov 14, 2011 11:04 pm

Re: Kiln Wash on Walls

Postby tgotch » Thu Jan 17, 2013 9:04 am

Kiln is level. I did have one roll slightly the other day. It did not touch the wall, but this is what caused me to worry about the walls.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Kiln Wash on Walls

Postby bob proulx » Thu Jan 17, 2013 12:09 pm

If there are no side elements I would go ahead, don't go any higher than you have too.
Bob

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Kiln Wash on Walls

Postby rosanna gusler » Thu Jan 17, 2013 1:27 pm

bottles will roll. they have a heavy side. i figure out which side that is and put a dot on the side that 'wants' to be up. i will also put a tiny piece of balled up used fiber under each side at the bottom. i shove it under with a paint brush. that said there is no reason why you could not wash the walls. rosanna
artist, owner of wanchese art studio, marine finisher

Arnold Howard
Posts: 45
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: Kiln Wash on Walls

Postby Arnold Howard » Mon Feb 11, 2013 6:08 pm

tgotch wrote:I have a paragon glass kiln with heating elements in the lid. I started slumping bottles, and am concerned about bottles rolling into the walls while firing. I put a small piece of thinfire under the sides, but still worry about rolling. Can I put kiln wash on the walls in case the bottles were to come in contact with them? I was reading Paragon's FAQ which states do not put kiln wash on walls, but it appears this may be referring to a kiln with elements in the walls. Thoughts?


You're right--the FAQ referred to kilns that have sidewall elements. If you are concerned that a bottle will roll against a wall in a kiln that has only lid elements, then it would be okay to kiln-wash the walls. Coat only as high up the wall as necessary, however.

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com

GuyKass
Posts: 75
Joined: Tue Jul 15, 2008 9:53 pm

Re: Kiln Wash on Walls

Postby GuyKass » Tue Feb 12, 2013 10:40 am

Cheap Insurance...

If you have the room, "strategically" place kiln furniture (or pieces of brick, pieces of tile, whatever) stuff along the edges of your shelf.

Obviously keep them out of the way of the slumping bottles, but if anything rolls, that will stop them from going overboard.

(Which of course does not really answer the question of kilnwashing the walls, but I guess I too, like the sound of my own voice.)


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 16 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com

cron