I am trying to break wine bottles to get large chunks of glass to do some fusing. I have recently tried to wrap the bottle in a plastic bag, and strike it with a hammer. The result more shattering, with a lot of small pieces, and very few large pieces.

Any ideas of how I can break these bottles and get larger pieces of glass?

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Ideas for Breaking Bottles

Postby Valerie Adams » Thu Sep 05, 2013 10:34 am

Looking at your website, it appears you must be using a tile saw to cut bottles. Can't you just chop them up in bigger sizes with your saw?

tgotch
Posts: 36
Joined: Mon Nov 14, 2011 11:04 pm

Re: Ideas for Breaking Bottles

Postby tgotch » Thu Sep 05, 2013 11:03 am

Valerie Adams wrote:Looking at your website, it appears you must be using a tile saw to cut bottles. Can't you just chop them up in bigger sizes with your saw?


I could, but that is a bit time consuming, plus I am looking for more of a "broken" look.

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Ideas for Breaking Bottles

Postby Brock » Thu Sep 05, 2013 11:21 am

Score. Tap. Break . . .

Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: Ideas for Breaking Bottles

Postby Laurie Spray » Fri Sep 06, 2013 12:15 am

Would it work tomheat it in the kiln then dunk into a bucket of cold water?? Never tried it but might be interesting.........
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Ideas for Breaking Bottles

Postby Morganica » Fri Sep 06, 2013 2:10 am

As Brock said. Make a few random scores on the clean bottle, then stick it in your plastic bag and whack it with the hammer. It'll still break, but the scores will relieve some of the shattering.

You could also try dropping it on a corner of a concrete stair from about 3 feet up. When I do that the bottle always breaks, and there goes the wine...
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Tom Fuhrman
Posts: 179
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: Ideas for Breaking Bottles

Postby Tom Fuhrman » Fri Sep 06, 2013 10:24 am

also try scoring and then put in a box and hit it with a sharp flame from a torch. It should give you nice larger pieces.

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Ideas for Breaking Bottles

Postby bob proulx » Fri Sep 06, 2013 4:46 pm

Tom Fuhrman wrote:also try scoring and then put in a box and hit it with a sharp flame from a torch. It should give you nice larger pieces.

That' how I do it.
Bob

Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Ideas for Breaking Bottles

Postby Peter Angel » Sat Sep 07, 2013 9:11 pm

Hitting it with a hammer is applying too much force.

Try putting it in a plastic bag, tying a knot in the plastic bag, and dropping it from a moderate height onto a hard surface eg stand on a chair and drop it on it's side onto concrete.
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.

rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Ideas for Breaking Bottles

Postby rosanna gusler » Sun Sep 08, 2013 3:09 pm

Torch
artist, owner of wanchese art studio, marine finisher

Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Ideas for Breaking Bottles

Postby Brock » Sun Sep 08, 2013 3:33 pm

"Hitting it with a hammer is applying too much force."

That might just depend how hard you hit it, doncha think?

Kevin Midgley
Posts: 713
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Ideas for Breaking Bottles

Postby Kevin Midgley » Sun Sep 08, 2013 4:21 pm

Isn't doncha think the sound of a correctly scored and struck bottle breaking? :lol:

Tammy Macdonald
Posts: 15
Joined: Tue Jun 18, 2013 1:45 pm
Location: Texas

Re: Ideas for Breaking Bottles

Postby Tammy Macdonald » Mon Sep 09, 2013 11:06 am

Kevin Midgley wrote:Isn't doncha think the sound of a correctly scored and struck bottle breaking? :lol:


I'd guess the correct spelling would be -- doncha TINK :roll:

Tod
Posts: 36
Joined: Tue Feb 14, 2006 5:47 pm
Location: Massachusetts

Re: Ideas for Breaking Bottles

Postby Tod » Wed Sep 11, 2013 11:21 am

For fun & in the name of science, you could also try lighting up your propane torch and hit the bottle with the flame...
Maybe fry it in a pan like we used to do with marbles?
please visit Beall Glass Studio on Face Book


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 8 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com