I have been testing Primo Primer, and like the results. One thing I have noticed though, is the primer tends to "muck" up in my storage container. I mix it in an old Gatorade bottle, put the marbles in it, and shake it up well. If it sits for longer than a day, the primer separates from the water a bit, and mucks up in the bottom.

Any way to avoid this?

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Primo Primer Muck

Postby Valerie Adams » Fri Oct 18, 2013 9:51 am

I keep Bullseye's primer pre-mixed in a bottle too and it also separates. I just shake well before using. The ingredients are too heavy to stay suspended in water.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Primo Primer Muck

Postby Bert Weiss » Sun Oct 20, 2013 3:15 pm

There is a primary difference between Bullseye primer and Primo primer. In Bullseye the binder is kaolin EPK clay. In Primo the binder is an organic gum. These materials behave differently in the way they mix and disperse.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

jim simmons
Posts: 459
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Primo Primer Muck

Postby jim simmons » Fri Oct 25, 2013 12:40 pm

Yea, but you can't avoid the separation
Jim


Bert Weiss wrote:There is a primary difference between Bullseye primer and Primo primer. In Bullseye the binder is kaolin EPK clay. In Primo the binder is an organic gum. These materials behave differently in the way they mix and disperse.

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Primo Primer Muck

Postby Morganica » Fri Oct 25, 2013 4:58 pm

Bullseye primer separates just as nicely. I have both, side by side on a shelf, not much difference in appearance except for color.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Primo Primer Muck

Postby Bert Weiss » Sun Oct 27, 2013 10:25 am

Kaoilin based primers are easier to remix than gum based.
Bert



Bert Weiss Art Glass*

http://www.customartglass.com

Furniture Lighting Sculpture Tableware

Architectural Commissions


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 3 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com