Re: Sticky cabochons: shelf paper vs kiln wash again

Postby Buttercup » Sun Jan 26, 2014 1:45 am

charlie wrote:
Morganica wrote:I do much the same thing with plaster of paris. I tend to use a broad spackling knife to flatten mine, but a rolling pin is a cool idea.


i use a wine bottle with the neck cut off. no handles on the ends to run into the kiln walls.


Charlie, doesn't the wine leak out? Jen

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Re: Sticky cabochons: shelf paper vs kiln wash again

Postby Lauri Levanto » Sun Jan 26, 2014 9:46 am

For some works where I have considered the back side critical, I have"casted"
the kiln wash.

I take a sheet of float glass, clean it and apply car wax which I polish carefully.
Then I cast a layer of gypsum. It will get an almost glossy surface. There gypsum plates i use for carving a pattern I want ti "print" on glass.

For minor works like cabochons, I also use a float glass as amould. I paint it with thick kilnwash, with a rolling pin press a 2-3 mm fiber paper into the wet kilnwash. Then i let it dry and peel the fiber paper carefully off. It leaves a nice
surface although it odten sticks into piece. Soaking overnight in a dilute phosphoric acid like Cocacola softens the contamination and it is easy to wash off.

-lauri

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Sticky cabochons: shelf paper vs kiln wash again

Postby Morganica » Sun Jan 26, 2014 4:56 pm

Fascinating, Lauri. Although I must admit that the first thing I thought was, "And we DRINK Cocacola?"

;-)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Lauri Levanto
Posts: 270
Joined: Tue Mar 11, 2003 7:33 am
Location: Halikko, Finland

Re: Sticky cabochons: shelf paper vs kiln wash again

Postby Lauri Levanto » Mon Jan 27, 2014 11:59 am

Morganica wrote:"And we DRINK Cocacola?"


So do I, too.
And I even smoke tobacco.
There are plenty of dangerous stuff we consume, chili for example.
They kill slowly, but I am retired, no need to hurry.

Ps.
The decalcinating stuff used for kitchenware is much cheaper.

jim simmons
Posts: 453
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Sticky cabochons: shelf paper vs kiln wash again

Postby jim simmons » Wed Jan 29, 2014 5:05 pm

Also white vinegar works just fine
Jim


Lauri Levanto wrote:For some works where I have considered the back side critical, I have"casted"
the kiln wash.

I take a sheet of float glass, clean it and apply car wax which I polish carefully.
Then I cast a layer of gypsum. It will get an almost glossy surface. There gypsum plates i use for carving a pattern I want ti "print" on glass.

For minor works like cabochons, I also use a float glass as amould. I paint it with thick kilnwash, with a rolling pin press a 2-3 mm fiber paper into the wet kilnwash. Then i let it dry and peel the fiber paper carefully off. It leaves a nice
surface although it odten sticks into piece. Soaking overnight in a dilute phosphoric acid like Cocacola softens the contamination and it is easy to wash off.

-lauri


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: Google [Bot], Majestic-12 [Bot] and 2 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com