Page 1 of 1
Super Spray Streaking
Posted: Mon Jan 27, 2014 11:29 am
by tgotch
I have been testing Super Spray A for my bottle devit issues (I usually use Borax concoction with fair success).
I brush on Super Spray with a foam brush, then fire to 1430. The gloss looks good, but the bottles have brush streaks in the glass after firing.
Anyone have suggestions to eliminate the streaks?
Re: Super Spray Streaking
Posted: Mon Jan 27, 2014 4:51 pm
by vblue
Go to Michael's or a craft store or art store and get a Badger air brush kit. Makes it a lot easier to use and no streaks. Helps to have a 40% off coupon for Michael s too.
Re: Super Spray Streaking
Posted: Wed Jan 29, 2014 12:52 am
by Laurie Spray
Spray for sure!
Re: Super Spray Streaking
Posted: Wed Jan 29, 2014 10:36 pm
by tgotch
Thanks for the tip. I bought a Badger 250-2 with a compressed air can to try (whole setup cost me ~$30 with coupon from Michaels.).
Results were much better.
I Just need a bit more practice to get more proficient with using the airbrush.
Re: Super Spray Streaking
Posted: Thu Jan 30, 2014 1:00 am
by Valerie Adams
And make sure you're shaking the container frequently. Using a brush means you're probably picking up more of the glass in the bottom of your container.