Best to put frit between 2 layers or on top?

Post by Shelley Lewis »

I want to use a green translucent base, a clear cap, and use black opal frit (medium) for some detail elements. Where is the best place for the frit? This will be a full fuse and later slumped.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Best to put frit between 2 layers or on top?

Post by Brock »

On top . . .
Shelley Lewis
Posts: 73
Joined: Wed Dec 11, 2013 11:14 am

Re: Best to put frit between 2 layers or on top?

Post by Shelley Lewis »

Thanks!