Searching for 4 pound containers of system 96 frit - WarmGlass.com

Searching for 4 pound containers of system 96 frit

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Shelley Lewis
Posts: 73
Joined: Wed Dec 11, 2013 11:14 am

Searching for 4 pound containers of system 96 frit

Postby Shelley Lewis » Tue Mar 11, 2014 2:55 pm

I'm having trouble finding 4 pound containers online, with the exception of clear frit. I want colors in the 4 pound size. Any suggestions? Thanks!

JestersBaubles
Posts: 696
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Searching for 4 pound containers of system 96 frit

Postby JestersBaubles » Tue Mar 11, 2014 3:03 pm

D&L Art Glass sells 4 lb jars, but you need a wholesale account.

Dana W.

Shelley Lewis
Posts: 73
Joined: Wed Dec 11, 2013 11:14 am

Re: Searching for 4 pound containers of system 96 frit

Postby Shelley Lewis » Tue Mar 11, 2014 3:08 pm

Sorry, forgot to mention I don't have a wholesale account

lorimendenhall
Posts: 91
Joined: Wed Apr 10, 2013 8:54 pm
Location: Orange County, CA
Contact:

Re: Searching for 4 pound containers of system 96 frit

Postby lorimendenhall » Tue Mar 11, 2014 3:59 pm

I'd ask Spectrum who their resellers are. they will be glad to help you buy their product!

Jenna
Posts: 46
Joined: Mon May 21, 2012 10:34 am

Re: Searching for 4 pound containers of system 96 frit

Postby Jenna » Tue Mar 11, 2014 4:31 pm

C R and Loo. They have some of the best prices, all the colors and good customer service. If they dont have the color in stock, they will order it for you. And you don't need a wholesale account.

beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: Searching for 4 pound containers of system 96 frit

Postby beninfl » Tue Mar 11, 2014 5:16 pm

http://www.franklinartglass.com/shop/ca ... /frit/122/

An excellent store, too, might I add!

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Searching for 4 pound containers of system 96 frit

Postby bob proulx » Wed Mar 12, 2014 8:20 am

I think Slumpy's sell five pound bags of 96 frit but it is not Spectrum's, I think it's Carolina frit.
Bob

beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: Searching for 4 pound containers of system 96 frit

Postby beninfl » Wed Mar 12, 2014 2:23 pm

bob proulx wrote:I think Slumpy's sell five pound bags of 96 frit but it is not Spectrum's, I think it's Carolina frit.
Bob


The Carolina Frit bags I have here in the shop have stickers on the box saying "Made from System 96 Glass". I believe that Slumpys just crushes the S96 glass and sorts/bags it themselves.

beninfl
Posts: 46
Joined: Sat Feb 08, 2014 8:54 pm

Re: Searching for 4 pound containers of system 96 frit

Postby beninfl » Wed Mar 12, 2014 2:27 pm

Image

bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Searching for 4 pound containers of system 96 frit

Postby bob proulx » Wed Mar 12, 2014 4:01 pm

Thanks Ben, that is good to know. I bought some before and I don't remember seeing Spectrum.
Bob

GuyKass
Posts: 75
Joined: Tue Jul 15, 2008 9:53 pm

Re: Searching for 4 pound containers of system 96 frit

Postby GuyKass » Fri Mar 14, 2014 2:40 pm

Call Kat at Uroboros. I am 100% sure she will work it out for you.

Guy

Shelley Lewis
Posts: 73
Joined: Wed Dec 11, 2013 11:14 am

Re: Searching for 4 pound containers of system 96 frit

Postby Shelley Lewis » Fri Mar 14, 2014 3:06 pm

Thanks for all the replies!

Jane Morgan
Posts: 28
Joined: Sat Sep 01, 2007 11:49 pm
Location: Central Coast of California

Re: Searching for 4 pound containers of system 96 frit

Postby Jane Morgan » Sun Mar 16, 2014 9:10 pm

Pacific Art Glass in Gardena, Ca has them.
Jane Morgan


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 12 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com