How to discover compatibility

Post by Linda D »

I have been *gifted* with a large amorphous shape of glass that is a LOT of dichroic fused onto black.
I can imagine cutting it up and remaking into something else.
Is there a way to test compatibility by fusing a test peice to something of known compatibility and checking for stress?
I think I know how to do, but would appreciate it if someone could wallk me though.
Thanks
Linda
Arnold Howard
Posts: 47
Joined: Mon Oct 13, 2003 5:21 pm
Location: Converse, Texas USA
Contact:

Re: How to discover compatibility

Post by Arnold Howard »

I don't think I would reuse the glass in a project. However, you might enjoy testing the glass for compatibility. Here are two articles that show how to use polarizing filters to test for stress. I experimented with filters and with polarizing sunglasses:

http://www.paragonweb.com/Kiln_Pointer.cfm?PID=403

http://www.paragonweb.com/Kiln_Pointer.cfm?PID=404

Sincerely,

Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / http://www.paragonweb.com
Linda D
Posts: 3
Joined: Sun Sep 30, 2007 11:53 pm

Re: How to discover compatibility

Post by Linda D »

Thanks!
L