Hello All,
I know that this color changes while being fired. It becomes grey instead of blue. It remains blue if it is capped, mostly with clear transparent glass, such as tekta 1108, or 1401.

I wonder if the same happens when I use powder 0146.
If I want the glass to remain steel blue - do I have to have to cap it? with clear transparent powder???

Many thanks,


Havi
PS is it possible perhaps to mix the 0146 with clear, to avoid the change of color???
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: BE 0146 Steel Blue - powder

Postby Terry Ow-Wing » Thu Jul 24, 2014 3:23 am

I want the opposite - if I use the steel blue powder uncapped will I get silver color where the powder is - even if it is a tiny line?
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image

suds
Posts: 34
Joined: Fri May 09, 2014 10:44 pm
Location: Sonoma County, CA

Re: BE 0146 Steel Blue - powder

Postby suds » Thu Jul 24, 2014 1:46 pm

I've never used BE0146 powder, but my limited experience with #2 & #3 frit is that firing in the 1450F - 1475F range is almost guaranteed to turn it grey (uncapped) but if you fire the hell out of it (>1500F) it will lose the grey and turn back to blue again.

I think Steel Blue is one of those colors where test samples are your best friend.
Steve

Havi
Posts: 589
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: BE 0146 Steel Blue - powder

Postby Havi » Thu Jul 24, 2014 5:38 pm

Thanks,
That's encouraging.



Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com

pshash
Posts: 45
Joined: Tue Dec 26, 2006 11:54 am
Location: Jacksonville, Florida
Contact:

Re: BE 0146 Steel Blue - powder

Postby pshash » Thu Jul 24, 2014 6:15 pm

I've used steel blue powder uncapped or capped and it stays blue.

Havi
Posts: 589
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: BE 0146 Steel Blue - powder

Postby Havi » Fri Jul 25, 2014 11:43 am

Thanks,

That's even MORE encouraging....
Have you used it on black background? Could you see it ???? This is what I basically plan, 0146 ON black sheet.



Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 5 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com