Sand corner of mold?

Postby Susanbuckler » Sun Dec 28, 2014 4:12 pm

Happy holidays to all
Finally have time to get back into my studio and I noticed a couple of the corners on BE molds are deteriorating slightly. Would you recommend sanding them a bit to even it out and then reapplying kiln wash ? Can I reapply kiln wash just to those spots or should I reapply it to the entire mold?
Thanks
Susan
Susan Buckler
Woodstock, NY

Vonon
Posts: 191
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Sand corner of mold?

Postby Vonon » Mon Dec 29, 2014 9:55 pm

I have done both of those things with no problem. Sometimes have managed to chip a little kiln wash off the rim and just repaired it with a dab of fresh kw and smoothed it with my finger. I guess it depends on how fanatic you might be about a smooth backside. :wink:
Vonon


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 12 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com