I see many questions about how to cut circles successfully, so I finally decided to write a blog post. My method is a little different than others. I hope some of you newer to fused glass find it useful.

http://jestersbaubles.blogspot.com/2015/02/cutting-glass-circles.html

Dana W.

Jerrwel
Posts: 129
Joined: Thu Feb 10, 2005 6:25 pm
Location: Charlotte, NC

Re: Circle cutting tutorial

Postby Jerrwel » Sat Feb 14, 2015 5:06 pm

JestersBaubles wrote:I see many questions about how to cut circles successfully, so I finally decided to write a blog post. My method is a little different than others. I hope some of you newer to fused glass find it useful.

http://jestersbaubles.blogspot.com/2015/02/cutting-glass-circles.html

Dana W.


Dana: Cutting off the corners of the square is brilliant! Will definately give your process a try on my next circle. Do you have a similar process for cutting rings? Would really like to be able to cut rings as a single piece; have you found that to be consistently possible?
Jerry

JestersBaubles
Posts: 689
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Circle cutting tutorial

Postby JestersBaubles » Sat Feb 14, 2015 5:57 pm

I cut rings the same way, but I won't say my success is consistent :mrgreen: . Sometimes they are perfect, and yep, other times they break (usually, just into two pieces, but sometimes more).

The saving grace is that typically I am cutting 2-3 rings of the same solid color, and so if you stagger the breaks when they are stacked, the breaks are not visible.

Dana W.


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 5 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com