I see many questions about how to cut circles successfully, so I finally decided to write a blog post. My method is a little different than others. I hope some of you newer to fused glass find it useful.

http://jestersbaubles.blogspot.com/2015/02/cutting-glass-circles.html

Dana W.

Re: Circle cutting tutorial

Posted: Sat Feb 14, 2015 5:06 pm
by Jerrwel
JestersBaubles wrote:I see many questions about how to cut circles successfully, so I finally decided to write a blog post. My method is a little different than others. I hope some of you newer to fused glass find it useful.

http://jestersbaubles.blogspot.com/2015/02/cutting-glass-circles.html

Dana W.


Dana: Cutting off the corners of the square is brilliant! Will definately give your process a try on my next circle. Do you have a similar process for cutting rings? Would really like to be able to cut rings as a single piece; have you found that to be consistently possible?

Re: Circle cutting tutorial

Posted: Sat Feb 14, 2015 5:57 pm
by JestersBaubles
I cut rings the same way, but I won't say my success is consistent :mrgreen: . Sometimes they are perfect, and yep, other times they break (usually, just into two pieces, but sometimes more).

The saving grace is that typically I am cutting 2-3 rings of the same solid color, and so if you stagger the breaks when they are stacked, the breaks are not visible.