I have a chance to buy an Evenheat GT 14-6 that someone is selling as a glass kiln with Rampmaster 2.
However, when I look at Evenheat's website, they describe the Rampmaster 2 for use in ceramic firing. Should I buy this kiln if I want to use it for glass?
Debbie
Evenheat with Rampmaster 2.. should I buy it?
Moderator: Tony Smith
-
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Evenheat with Rampmaster 2.. should I buy it?
The 14-6 is indeed a glass kiln and should be great for a beginner. The Rampmaster 2 is Evenheat's controller for both glass and ceramic kilns.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun