Evenheat with Rampmaster 2.. should I buy it?

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
DebB
Posts: 15
Joined: Tue Sep 02, 2014 11:04 pm

Evenheat with Rampmaster 2.. should I buy it?

Post by DebB »

I have a chance to buy an Evenheat GT 14-6 that someone is selling as a glass kiln with Rampmaster 2.
However, when I look at Evenheat's website, they describe the Rampmaster 2 for use in ceramic firing. Should I buy this kiln if I want to use it for glass?

Debbie
Debbie
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Evenheat with Rampmaster 2.. should I buy it?

Post by Tony Smith »

The 14-6 is indeed a glass kiln and should be great for a beginner. The Rampmaster 2 is Evenheat's controller for both glass and ceramic kilns.

Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
DebB
Posts: 15
Joined: Tue Sep 02, 2014 11:04 pm

Re: Evenheat with Rampmaster 2.. should I buy it?

Post by DebB »

Thanks Tony. I'm excited to try it. :)
Debbie