Doug Randall
Posts: 102
Joined: Sun Aug 17, 2003 10:11 pm
Location: Portland, OR
Contact:

Slumped glass form

Postby Doug Randall » Mon Jun 08, 2015 4:05 pm

We used to call them floppy bowls, rounds of glass places on top of a cylindrical SS form, like an old milkshake mixing container. What do you folks call the bowls they make. Haven't seen them in years.

carol carson
Posts: 56
Joined: Sat Jul 30, 2005 6:25 pm
Location: Portland OR
Contact:

Re: Slumped glass form

Postby carol carson » Mon Jun 08, 2015 6:50 pm

Doug,

I think they call them floral formers.

Marty
Posts: 851
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Slumped glass form

Postby Marty » Mon Jun 08, 2015 8:36 pm

Doug- you must not be getting out much.
The blowers call them handkerchief vases (blow a bubble, open it and spin it out then let it drape) but I've got another name for them that I can't use here.

Bert Weiss
Posts: 2337
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Slumped glass form

Postby Bert Weiss » Mon Jun 08, 2015 10:17 pm

Back in the 80's I paid $18 for a floral former from a glass wholesaler. Then I bought a martini shaker for $3.50 from a restaurant supply house. it turned out they were exactly the same, same manufacturer and everything.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions

Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Slumped glass form

Postby Morganica » Tue Jun 09, 2015 7:10 pm

The formal name for them is "fazzoletto" or "fazzoletto vase." But like Marty said, it means "handkerchief."
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)

Marty
Posts: 851
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Slumped glass form

Postby Marty » Wed Jun 10, 2015 10:28 pm

That wasn't the name I was thinking about....

DonMcClennen
Posts: 366
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Slumped glass form

Postby DonMcClennen » Fri Jun 12, 2015 5:34 pm

I think they are a novice piece produced following success making "coasters". We were all there at one time longgggggg ago!
"The Glassman"


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 5 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com