Pre-firing Stringers

Postby Jan de Jong » Sun Aug 30, 2015 5:14 am

Hello ! I wonder which simple quick schedule I can use to pre-fire Stringers to avoid rolling ? Jan de Jong

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Pre-firing Stringers

Postby Stephen Richard » Sun Aug 30, 2015 5:18 am

This is one method that does not need firing before use.
http://glasstips.blogspot.co.uk/2015/07 ... ngers.html
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/

Jan de Jong
Posts: 97
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Pre-firing Stringers

Postby Jan de Jong » Sun Aug 30, 2015 7:51 am

@ Steven Richard: Thank you for your answer, but is there a simple, quick firing-schedule known for this stringers ?? I have to do much stringers, so my choice is pre-firing. greetings from Holland, Jan

Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Pre-firing Stringers

Postby Valerie Adams » Sun Aug 30, 2015 5:29 pm

I guess you'd have to test for your kiln, but when I slump stringer, I fire afap to 1250° and hold until visually confirmed. If you're trying for a flat side, you'd probably have to fire a little hotter.

I'd choose a temp to start with and monitor them. When they should be done, quickly remove one with a long needle nosed plier (and gloves!), and check it. Add time as necessary.

Jerrwel
Posts: 129
Joined: Thu Feb 10, 2005 6:25 pm
Location: Charlotte, NC

Re: Pre-firing Stringers

Postby Jerrwel » Mon Aug 31, 2015 11:41 am

Liquid Stringer Medium advertisement makes this claim, 'Its primary benefit is that it will withstand elevated temperatures thus holding the glass particles in place until they are sticky enough to bond together on their own.' This seems to indicate that you can use this product to tack the stringers in place and fire while the Liquid Stringer Medium holds the the stringers in place.

I have used the product for other purposes and find that it does burn off clean.
Jerry

Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Pre-firing Stringers

Postby Stephen Richard » Mon Aug 31, 2015 4:45 pm

OK. As fast as possible to 740C, off
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/

Jan de Jong
Posts: 97
Joined: Sun Mar 09, 2003 3:31 pm
Location: The Netherlands

Re: Pre-firing Stringers

Postby Jan de Jong » Fri Sep 04, 2015 9:13 am

Okay.....thank you all for your respons ! greetings from Holland, Jan de Jong


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 9 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com