How to adhere stand up project to a glass base

Post by LCS »

What is the best method and glue to adhere a stand up glass project to a glass base?
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: How to adhere stand up project to a glass base

Post by JestersBaubles »

Depends upon the shape of the glass you are gluing to the base. If it has some means of support in its inherent design, you could use something as simple as E6000. I recently wrote a blog post on a candle shield, that might be helpful:

http://jestersbaubles.blogspot.com/2016 ... hield.html

If the glass piece can't support itself very well against gravity :mrgreen: I would use something like HXTAL.

Dana W.
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: How to adhere stand up project to a glass base

Post by DonMcClennen »

Glass to glass.. use UV adhesive
"The Glassman"