helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Disposing of ground glass

Postby helenM » Fri Sep 02, 2016 6:06 am

Hi, I've just bought a diamond pad to grind some glass edges before fire polishing (and to learn how to use it - just bought Paul Tarlow's book to help, excellent book) but I was wondering what the best way of disposing the waste glass is. I thought I would do the grinding in water, let it settle then drain of what water I could and throw the rest in a plastic bag and wrap up for throwing away in my normal waste.

What do other people do when coldworking? I live in the UK so I'm not sure if there are any rules about this (may have to do a bit of research on that). Also I like to be as ecofriendly as possible when disposing of waste craft products.

jim burchett
Posts: 217
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Disposing of ground glass

Postby jim burchett » Fri Sep 02, 2016 4:39 pm

I,personally do not consider ground glass as a hazard to anything but plumbing. I treat it as I would diatomaceous earth and spread it around plants in the garden.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie

JestersBaubles
Posts: 669
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Disposing of ground glass

Postby JestersBaubles » Fri Sep 09, 2016 11:55 am

Ditto. Pour it on the plants.

Dana W.

helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Re: Disposing of ground glass

Postby helenM » Fri Sep 16, 2016 11:38 am

Thank you!

Ed Cantarella
Posts: 146
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Disposing of ground glass

Postby Ed Cantarella » Tue Mar 13, 2018 8:38 pm

Just run it down the largest drain in the house - probably the toilet. Seriously - you've probably washed larger grains of sand off vegetables from the store.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

Buttercup
Posts: 515
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Disposing of ground glass

Postby Buttercup » Thu Mar 15, 2018 11:18 pm

DON'T put it down the toilet if you have a worm-powered sewage system. It'll tear their little guts out!

Marty
Posts: 833
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Disposing of ground glass

Postby Marty » Fri Mar 16, 2018 10:59 am

Don't put it down ANY drain.

Ed Cantarella
Posts: 146
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Disposing of ground glass

Postby Ed Cantarella » Fri Mar 16, 2018 11:21 am

Marty wrote:Don't put it down ANY drain.
OP is only talking a little powder - what's the harm? Glass is sand(roughly), sand is glass. We all habitually wash dirty clothing with embedded sand down the drain and same for dirty vegetables,dogs, etc. And we eat a fair amount which comes out . . :mrgreen: . https://health.howstuffworks.com/wellne ... t-year.htm

But I would fully agree that one shouldn't dump grinder sludge down a drain - the particles are much too large to be carried away and could start to accumulate in the trap (u-shaped piece on the drain pipe).
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.

Terry Crider
Posts: 10
Joined: Mon Jul 25, 2005 4:17 pm
Location: Western Ohio

Re: Disposing of ground glass

Postby Terry Crider » Mon Mar 19, 2018 11:03 am

Any thoughts on washing very small brushes out in the bath room sink --- Brad's and Barry K's "paints"

Barry Kaiser
Posts: 261
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Disposing of ground glass

Postby Barry Kaiser » Mon Mar 19, 2018 8:59 pm

Terry,
The politically sensitive answer is to not do so.
I did it all the time. Our paints contain very little (relatively) solids and those are ultra fine.
However, I have now installed a Gleko Trap since I do a lot (and I mean a lot) of painting and washing. After the first year, I cleaned out the trap and it was amazing how little solids there was.

Barry

JestersBaubles
Posts: 669
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Disposing of ground glass

Postby JestersBaubles » Tue Mar 20, 2018 11:02 pm

I have a Gleco trap on my utility sink. I wash anything glass related in that sink (glass itself, brushes, etc). If the piece is small enough, I'll coldwork with handpads in that sink. The grinder sludge, I scrape out and dispose of. Other coldworking water usually ends up in the yard (the water bucket for the lap grinder & saw).

The utility sink is also great for washing dirty vegetables :) .

Dana


Post Reply

Return to “Newcomer Forum”

Who is online

Users browsing this forum: No registered users and 2 guests

Warm Glass

2575 Old Glory Road, Suite 700
Suite 700
Clemmons, NC 27012
Phone: (336) 712 8003
Email: wg@warmglass.com